To get a PDF copy, press Print and choose “Save as PDF”.

FRP Deformed Rebar Technical Data Sheet — Structural GFRP Rebar and Fiberglass Reinforcing Bar by NABAK COMPOSITE

Cover of the NABAK COMPOSITE FRP deformed rebar technical data sheet – FRP / GRP Deformed Rebar, code NBK-TDS-DRB-01-EN
FRP / GFRP Deformed Rebar — Technical Data SheetIntroduction, rib types and benefits | Page 1 of 5

NABAK COMPOSITE FRP deformed rebar (FRP / GRP Deformed Rebar) is a structural GFRP bar for reinforcing concrete. A helical or moulded rib and an optional sand coating give it full mechanical bond with concrete. It does not rust, has about twice the tensile strength of steel rebar at one quarter of the weight, is non-magnetic and electrically insulating, and extends the service life of concrete structures in corrosive environments many times over.

Ø 6 – 32 mmFRP deformed rebar diameters
≥ 7.6 MPaBond to concrete (ASTM D7957)
≥ 44.8 GPaTensile modulus of elasticity
ACI 440Structural design basis

What is FRP deformed rebar (ribbed GFRP rebar)?

FRP deformed rebar, also known as composite rebar, FRP rebar, GFRP rebar, fiberglass rebar, composite reinforcement and ribbed FRP bar, is made by pultruding continuous glass-fibre rovings impregnated with vinyl ester or epoxy resin. Before full cure, a helical rib is wound around the core or moulded ribs are formed, and the surface can be coated with silica sand; the GFRP bar is then cured in a heated tunnel.

FRP is the general name for fibre-reinforced polymers, and GFRP (or GRP) is FRP made with glass fibre. The surface rib is the main difference between deformed FRP rebar and smooth bar: through mechanical interlock and friction, the ribs transfer tensile force from the concrete into the fibre core, making the bar suitable as main reinforcement in beams, slabs, walls and columns in accordance with ASTM D7957, CSA S807 and ACI 440.

Surface and rib types of composite rebar

Helical wrapA fibre strand wound around the core forms a continuous spiral rib; the most common deformed GFRP rebar.
Moulded ribTransverse ribs formed in a mould, similar in appearance to deformed steel rebar.
Sand-coatedSilica grains bonded to the surface increase roughness, chemical bond and friction.
Rib + sandHelical rib combined with sand coating for the highest bond of FRP rebar to concrete.

Benefits of deformed FRP rebar in concrete

  • No reinforcement corrosion: composite rebar does not rust in chlorides, sulphates, carbonation or seawater, so rust-induced cracking and spalling of concrete are eliminated.
  • Less cover and fewer admixtures: thick concrete cover, silica fume and corrosion inhibitors are needed less.
  • Lightweight: GFRP rebar is about 70% lighter than steel; faster, safer handling and fixing.
  • High tensile strength: 700 – 1100 MPa, two to three times the yield stress of steel rebar.
  • Non-magnetic and insulating: suited to substations, railways, MRI rooms, airports and field-sensitive structures.
  • Cuttable by TBM: composite reinforcement in tunnel launch and reception walls (soft-eye) can be cut by the boring machine.

Production steps of deformed GFRP rebar

  1. Roving feed: dozens of alkali-resistant ECR glass rovings are fed from the creel into the composite rebar line.
  2. Impregnation: the fibres are fully wetted in a vinyl ester or epoxy resin bath and excess resin is removed.
  3. Core forming: the fibres pass through a round die and the FRP rebar core is formed to an accurate diameter.
  4. Rib forming: the rib strand is wound helically around the core, or the rib is formed in a mould.
  5. Sanding and curing: where required, silica sand is applied and the GFRP bar is cured in a heated tunnel.
  6. Cutting and control: the deformed bar is cut to order length and its diameter, weight, Tg and tensile strength are checked.
FRP / GFRP Deformed Rebar — Technical Data SheetDiameters, dimensions, bends and applications | Page 2 of 5

Diameter and specification table of deformed composite rebar

Table 1 — Deformed GFRP rebar specifications (ρ ≈ 2.1 g/cm³, E ≥ 50 GPa)
Nominal diameter (mm)Imperial equivalentNominal area (mm²)Approx. weight incl. ribs (g/m)Guaranteed tensile strength ffu* (MPa)Guaranteed tensile force (kN)Rib height (mm)
6#228.365 – 701100310.4 – 0.6
8—50.3115 – 1251050530.5 – 0.8
10#378.5180 – 1951000790.6 – 0.9
12#4113.1240 – 2609501070.7 – 1.0
14—153.9330 – 3559201420.8 – 1.1
16#5201.1430 – 4509001810.9 – 1.2
18—254.5545 – 5808802241.0 – 1.3
20#6314.2675 – 7108502671.0 – 1.4
22#7380.1815 – 8608303151.1 – 1.5
25#8490.91050 – 11108003931.2 – 1.6
28#9615.81320 – 13907504621.3 – 1.7
32#10804.21720 – 18107005631.4 – 1.8

Per ASTM D7957, the actual cross-sectional area of deformed composite rebar is measured by immersion and must fall within the permitted range of the nominal area; the weight is higher than smooth bar because of the ribs and sand. Imperial equivalents are approximate. The guaranteed strength of each order is determined by ASTM D7205 testing.

Bent bars, stirrups and spirals in composite rebar

Table 2 — Prefabricated GFRP shapes (bent in the factory, before cure)
ShapeApplicationMinimum inside bend radiusStrength at the bend
L-bar (90° hook)End anchorage, slab-to-wall connection3 db≈ 0.45 ffu (Formula 13)
U-barSlab edges, column heads, transverse anchorage3 db≈ 0.45 ffu
Closed and open stirrupsShear reinforcement of beams and columns3 db≈ 0.45 ffu
SpiralRound columns and pilesTo orderBy testing

Cured composite rebar cannot be bent on site; the bar bending schedule must be submitted before production. Standard straight bar lengths are 6 and 12 m.

Applications of deformed composite rebar

Coastal and marine structuresJetties, breakwaters, sea walls and structures in contact with seawater
Bridges and bridge decksDeck slabs, parapets and slabs exposed to de-icing salts, reinforced with GFRP rebar
Car parks and industrial floorsMulti-storey car park slabs and floors exposed to chlorides and chemicals
Treatment plants and tanksBasins, sewage tanks and concrete channels with composite reinforcement
Tunnels and metroSoft-eye walls, segment elements and structures cut by TBM
Non-magnetic structuresSubstations, transformer foundations, MRI rooms and navigation platforms
FRP / GFRP Deformed Rebar — Technical Data SheetProperties, standards and comparison | Page 3 of 5

Properties of deformed GFRP rebar and ASTM D7957 requirements

Table 3 — Reference properties of deformed composite rebar compared with ASTM D7957 minimums
PropertyTest methodTypical value, deformed FRP rebarASTM D7957 requirement
Glass fibre content (by weight)ASTM D2584 / D317175 – 82%≥ 70%
Tensile modulus of elasticityASTM D720550 – 60 GPa≥ 44.8 GPa
Ultimate strainASTM D72051.4 – 2.2%—
Bond strength to concreteASTM D791310 – 16 MPa≥ 7.6 MPa
Transverse shear strengthASTM D7617150 – 200 MPa≥ 131 MPa
Moisture absorptionASTM D570≤ 0.2%≤ 0.25% (and ≤ 1% at saturation)
Glass transition temperature TgASTM E1356 / E1640105 – 130 °C≥ 100 °C
Degree of resin cureASTM E2160≥ 95%≥ 95%
Coefficient of expansion, longitudinal / transverseASTM E8316 – 10 / 21 – 30 ×10⁻⁶ /°C—
Alkali durability (strength retention)ASTM D7705≥ 80%Per project specification

Values are typical ranges of the FRP and GFRP composites industry and are not NABAK COMPOSITE’s own laboratory results. Other related standards: CSA S807 (FRP rebar specification), ACI 440.1R-15 (design guide), ACI CODE-440.11 (building code for GFRP-reinforced concrete) and ACI 440.3R (test methods).

Deformed FRP rebar compared with steel rebar

Table 4 — Deformed composite rebar vs S400 steel, epoxy-coated steel and smooth FRP bar
FeatureDeformed GFRP rebarS400 steelEpoxy-coated steelSmooth FRP bar
Tensile strength (MPa)700 – 1100Yield 400Yield 400700 – 1100
Modulus (GPa)50 – 6020020050 – 55
Bond to concreteHigh (rib + sand)High10 – 20% lowerLow
Structural concrete reinforcementSuitable (ACI 440)SuitableSuitableNot suitable
CorrosionNoneSevere in chloridesAt coating damageNone
Behaviour up to failureElastic, no yieldingDuctileDuctileElastic
Bending on siteNot possibleEasyWith careNot possible

Different design, not one-for-one replacement: deformed composite rebar does not yield and its modulus is about one quarter of steel; design of FRP-reinforced concrete is therefore usually governed by crack, deflection and creep-rupture checks (serviceability), and sections are deliberately designed “over-reinforced” so that failure occurs by concrete crushing. The formulas on pages 4 and 5 are based on ACI 440.1R-15.

Concrete cover and fire protection of composite rebar

Table 5 — Concrete cover guidance for deformed FRP rebar
Member conditionRecommended coverRemarks
Interior slabs and walls≥ db and ≥ 20 mmPrevents longitudinal splitting from the transverse expansion of GFRP rebar
Interior beams and columns≥ 30 – 40 mm≥ 30 – 40 mm
Exposed to earth or weather≥ 40 – 50 mmBenefit: the thick anti-corrosion cover needed for steel is no longer required
Fire-resistance requirementPer the project fire rating, typically ≥ 50 – 60 mmComposite rebar temperature at anchorage zones must stay below Tg
FRP / GFRP Deformed Rebar — Technical Data SheetFlexural design per ACI 440.1R | Page 4 of 5

Flexural strength formulas for FRP-reinforced concrete

1. Design strength of the bar
ffu = CE · ffu*

CE = 0.8 for interior concrete and 0.7 for concrete exposed to earth or weather. ffu* = 800 → ffu = 560 MPa

2. Balanced reinforcement ratio
ρfb = 0.85 β1 f′cffu · Ef εcuEf εcu + ffu

f′c = 30, β₁ = 0.85, Ef = 50 GPa, εcu = 0.003 → ρfb ≈ 0.0082

3. Bar stress in an over-reinforced section (ρf > ρfb)
ff = √( (Ef εcu)²4 + 0.85 β1 f′cρf Ef εcu ) − 0.5 Ef εcu ≤ ffu

Failure by concrete crushing; the composite rebar remains below its ultimate strength.

4. Nominal moment and strength reduction factor
Mn = ρf ff ( 1 − 0.59 ρf fff′c ) b d²

φ = 0.55 for ρf ≤ ρfb; φ = 0.3 + 0.25 ρf/ρfb in the transition zone; φ = 0.65 for ρf ≥ 1.4 ρfb

Design example — 200 mm one-way slab with deformed GFRP Ø16 at 125 mm (1 m width)
d = 160 mm ; Af = 201.1 × 1000/125 ≈ 1609 mm²/m ; ρf = 1609 / (1000 × 160) ≈ 0.0101 ρf / ρfb = 0.0101 / 0.0082 ≈ 1.23 → transition zone → φ = 0.3 + 0.25 × 1.23 ≈ 0.61 Ef εcu = 150 MPa → ff = √(150²/4 + 0.85×0.85×30/0.0101 × 150) − 75 ≈ 499 MPa ≤ 560 ✓ Mn = 0.0101 × 499 × (1 − 0.59 × 0.0101 × 499 / 30) × 1000 × 160² ≈ 115.7 kN·m/m φ Mn ≈ 0.61 × 115.7 ≈ 70.3 kN·m/m The section is over-reinforced and failure is controlled by concrete crushing — the desired behaviour for concrete reinforced with composite rebar. Serviceability checks of this slab continue on page 5.
5. Sustained stress limit (creep rupture) and concrete shear strength
ff,s ≤ 0.20 ffu ,    Vc = 0.4 √f′c · bw · c ,   c = k d

In the example: ff,s ≤ 0.2 × 560 = 112 MPa; k ≈ 0.179 → c ≈ 28.6 mm → Vc ≈ 0.4 × 5.48 × 1000 × 28.6 ≈ 62.8 kN/m. The concrete shear contribution in FRP-reinforced sections is lower than with steel because the compression zone is shallower.

6. Minimum flexural reinforcement (under-reinforced section)
Af,min = 0.41 √f′cffu bw d ≥ 2.26ffu bw d

Required only when ρf < ρfb, so that the FRP bar does not rupture after cracking.

7. Temperature and shrinkage reinforcement
ρf,ts = 0.0018 × 414ffu × EsEf ,   0.0014 ≤ ρf,ts ≤ 0.0036

ffu = 560, Ef = 50 GPa → 0.0053 → capped at 0.0036; 200 mm slab: A = 720 mm²/m → GFRP Ø12 at 150 mm

FRP / GFRP Deformed Rebar — Technical Data SheetServiceability, development length and installation | Page 5 of 5

Crack, deflection and development length formulas for FRP rebar

8. Neutral axis depth of the cracked section
k = √( 2ρf nf + (ρf nf)² ) − ρf nf ,   nf = EfEc

Ec = 4700√f′c ≈ 25.7 GPa → nf ≈ 1.94 → k ≈ 0.179

9. Bar stress under service load
ff,s = MsAf · d (1 − k/3)

Ms = 25 kN·m/m → ff,s ≈ 103 MPa ≤ 112 MPa (creep limit) ✓

10. Crack width (ACI 440.1R)
w = 2 ff,sEf β kb √( dc² + (s/2)² )

β ≈ 1.30, kb = 1.4, dc = 40, s = 125 → w ≈ 0.56 mm ≤ 0.7 mm (interior limit) ✓; the exterior limit is 0.5 mm: spacing 100 mm → w ≈ 0.39 mm ✓

11. Effective moment of inertia (Bischoff)
Ie = Icr1 − γ (Mcr/Ma)² (1 − Icr/Ig)

γ = 1.72 − 0.72 Mcr/Ma. In the example: Icr ≈ 6.2×10⁷, Ig ≈ 6.7×10⁸ mm⁴, Mcr ≈ 22.6 kN·m → Ie ≈ 3.0×10⁸ mm⁴

12. Development length of a straight bar
ld = α ( ffr0.083 √f′c − 340 )13.6 + C/db db ≥ 20 db

Ø16, ffr = 400 MPa, f′c = 30, C = 2db, α = 1 → ld ≈ 554 mm (≥ 320 mm)

13. Strength of the bar at a bend
ffb = ( 0.05 rbdb + 0.3 ) ffu ≤ ffu

rb = 3 db → ffb = 0.45 ffu; apply to composite stirrups and hooks.

Installation guide for deformed composite rebar

  1. Bending schedule: fix all bends, stirrups and lengths before production; GFRP rebar is not bent on site.
  2. Handling and storage: support on bearers at ≤ 2 m spacing, away from sunlight, and never drag on the ground.
  3. Cutting: cut with a diamond or abrasive disc and wear a mask and goggles; rebar shears must not be used.
  4. Tying: tie with coated wire, plastic ties or nylon wire; use plastic spacers to achieve the cover.
  5. Concrete cover: at least one bar diameter and not less than 20 – 25 mm; anchor the cage against flotation during pouring.
  6. Splices: lap splices with length ≥ 1.3 ld; welding and steel mechanical couplers are not applicable to composite rebar.
Request a quote for FRP deformed rebar: send diameters and quantities, the bending schedule, surface type (rib, sand or both), type of structure and service environment.
Nabak Saze Gostar | nabakcomposite.com | +98 21 4881 2124 | Mobile +98 912 396 3078 | Instagram @nabak.composite

Disclaimer: The information in this data sheet is based on general, typical data of the FRP and GFRP composites industry and the ACI 440 and ASTM D7957 standards, and is intended as guidance only. Design examples are for illustration; structural design with composite rebar must be carried out by a structural engineer. NABAK COMPOSITE reserves the right to change technical specifications without notice.