FRP Angle Profile Technical Data Sheet — Pultruded GFRP and Fiberglass Angle by NABAK COMPOSITE

Cover of the NABAK COMPOSITE FRP angle technical data sheet – FRP / GRP Angle Profile, code NBK-TDS-ANG-01-EN
FRP / GFRP Angle Profile — Technical Data SheetIntroduction, structure and applications | Page 1 of 5

NABAK COMPOSITE FRP angle (FRP / GRP Angle Profile) is a pultruded L-shaped GFRP profile with equal or unequal legs. Lightweight, rust-free, electrically insulating and paint-free, it is the most widely used connection, bracing and support member in composite structures, FRP grating platforms, cable trays and equipment in corrosive environments.

25 – 150 mmAngle leg width
3 – 12.7 mmLeg thickness
≥ 240 MPaLongitudinal tensile strength (E23)
≈ 1/4of the weight of an equal steel angle

What is FRP angle (GFRP angle profile)?

Composite angle, also known as FRP angle, GFRP angle, fiberglass angle, composite angle profile and pultruded angle, is made by continuously pulling glass-fibre rovings and transverse mats impregnated with resin through a heated L-shaped die. Continuous fibres around the corner ensure an integral connection of the two legs, and the surface veil protects the profile against UV and moisture.

FRP is the general name for fibre-reinforced polymers, and GFRP (or GRP) is FRP made with glass fibre. Composite angle is an open, asymmetric section: its principal axes are inclined, its torsional stiffness is low and in compression it is sensitive to torsional buckling. FRP angle is therefore used mainly for connections, tension bracing, supports and framing, while composite tube is a better choice for columns.

Structure and types of composite angle

Equal-leg angleTwo legs of equal width; the most common FRP angle for connections, bracing and framing.
Unequal-leg angleLong leg for higher stiffness in one direction; grating edge supports and cantilevers.
Integral cornerContinuous fibres and an inside corner radius that reduces stress concentration.
Surface veilSmooth, resin-rich surface for UV and chemical resistance and a uniform finish of GFRP angle.

Advantages of FRP angle over steel angle

  • Corrosion-resistant: composite angle does not rust in seawater, chlorine, acids or sewage; no galvanizing or painting.
  • Lightweight: a 50×50×5 GFRP angle weighs only 0.88 kg/m — about a quarter of an equal steel angle.
  • Electrically insulating: safety in substations, battery rooms and structures near live lines.
  • Non-magnetic and non-sparking: suited to explosive atmospheres and sensitive equipment.
  • Simple fabrication: cut with a diamond saw and bolted or bonded; no welding or hot work.
  • Compatible with FRP systems: same material as composite grating, handrail and tube in one structure.

Applications of FRP composite angle

Clip anglesBeam-to-column and beam-to-beam connections in composite tube and I-beam structures
Grating supportsEdge angles to seat FRP grating on concrete walls and beams
Bracing and trussesTension members and light bracing of platforms and cooling towers
Hatch and trench framesFrames for trench covers, inspection hatches and treatment-plant channels
Cable tray and panelsInsulating brackets, posts and frames in electrical installations
Edging and protectionWall-corner guards, stair nosings and equipment frames in corrosive areas
FRP / GFRP Angle Profile — Technical Data SheetSize and section property tables | Page 2 of 5

Equal-leg composite angle table

Table 1 — Equal-leg FRP angle: sizes and section properties (ρ = 1.85 g/cm³)
Size b×b×t (mm)A (mm²)Weight (kg/m)Centroid e (mm)Ix = Iy (mm⁴)Iu maximum (mm⁴)Iv minimum (mm⁴)iv (mm)J (mm⁴)
25 × 25 × 31410.267.48.20×10³1.30×10⁴3.38×10³4.9423
38 × 38 × 6.44450.8211.85.75×10⁴9.07×10⁴2.44×10⁴7.46.08×10³
40 × 40 × 43040.5611.54.61×10⁴7.34×10⁴1.88×10⁴7.91.62×10³
50 × 50 × 54750.8814.31.13×10⁵1.79×10⁵4.59×10⁴9.83.96×10³
50 × 50 × 6.45991.1114.81.38×10⁵2.20×10⁵5.72×10⁴9.88.18×10³
76 × 76 × 6.49321.7221.45.17×10⁵8.25×10⁵2.10×10⁵15.01.27×10⁴
76 × 76 × 9.513542.5022.57.25×10⁵1.15×10⁶2.99×10⁵14.94.07×10⁴
100 × 100 × 6.412392.2927.41.21×10⁶1.94×10⁶4.89×10⁵19.91.69×10⁴
100 × 100 × 9.518103.3528.51.72×10⁶2.74×10⁶7.01×10⁵19.75.44×10⁴
100 × 100 × 12.723794.4029.72.20×10⁶3.49×10⁶9.09×10⁵19.61.28×10⁵
150 × 150 × 9.527605.1141.06.08×10⁶9.71×10⁶2.45×10⁶29.88.30×10⁴

Unequal-leg composite angle table

Table 2 — Unequal-leg FRP angle: sizes and section properties
Size B×b×t (mm)A (mm²)Weight (kg/m)ey / ex (mm)Ix (mm⁴)Iy (mm⁴)Iv minimum (mm⁴)iv (mm)J (mm⁴)
76 × 50 × 6.47651.4225.3 / 12.34.50×10⁵1.57×10⁵9.05×10⁴10.91.05×10⁴
100 × 50 × 6.49191.7035.8 / 10.89.60×10⁵1.68×10⁵1.07×10⁵10.81.25×10⁴
100 × 76 × 9.515822.9331.9 / 19.91.57×10⁶7.88×10⁵4.19×10⁵16.34.76×10⁴
150 × 100 × 9.522854.2348.6 / 23.65.32×10⁶1.94×10⁶1.10×10⁶21.96.87×10⁴

e is the distance of the centroid from the back of the leg; u and v are the principal axes (at 45° for equal angles). Properties are calculated with the formulas on page 4 for a sharp corner; the actual corner radius changes the values slightly. Common market sizes of pultruded composite angle are supplied in 6 m lengths; tolerances per EN 13706-2.

Selection guide for composite angle by application

Table 3 — Recommended FRP angle for common applications
ApplicationRecommended angle (mm)Design note
Clip angle for 100 mm tube beam-to-column joint76 × 76 × 9.5 or 100 × 100 × 9.5Check transverse bending of the leg (Formula 12)
FRP grating edge support50 × 50 × 6.4 / 76 × 50 × 6.4Seat width ≥ 38 mm for grating
Platform tension bracing50 × 50 × 5 / 76 × 76 × 6.4Shear lag of single-leg connection (Formula 9)
Short compression brace76 × 76 × 9.5 or double angleTorsional and flexural buckling (Formula 8)
Hatch frames and channel covers40 × 40 × 4 / 50 × 50 × 5Framing with stainless or FRP bolts
Cable-tray bracket76 × 50 × 6.4 / 100 × 50 × 6.4Long leg in the load direction
Edging and corner guard25 × 25 × 3 / 38 × 38 × 6.4Bonded or riveted

Choosing thickness: in composite angle, the leg width-to-thickness ratio (b/t) matters more than overall size. Angles with b/t ≤ 8 (such as 50×50×6.4 and 76×76×9.5) perform much better in compression and connections than thin-walled angles, although they weigh slightly more per metre.

FRP / GFRP Angle Profile — Technical Data SheetMaterial properties, comparison and options | Page 3 of 5

Mechanical properties of composite angle (EN 13706 grade)

Table 4 — Reference properties of pultruded GFRP angle
PropertyTest methodEN 13706 grade E23 minimumTypical value, FRP angle
Longitudinal tensile modulus ELEN ISO 527-423 GPa23 – 28 GPa
Transverse modulus ETEN ISO 527-4—7 – 9 GPa
In-plane shear modulus GLT——3 – 4 GPa
Tensile strength, longitudinal / transverseEN ISO 527-4240 / 50 MPa250 – 350 / 50 – 80 MPa
Flexural strength, longitudinal / transverseEN ISO 14125240 / 100 MPa250 – 350 / 100 – 130 MPa
Longitudinal compressive strengthEN ISO 14126—240 – 300 MPa
Apparent shear strengthEN ISO 1413025 MPa25 – 35 MPa
Pin-bearing strength, longitudinal / transverseEN 13706150 / 70 MPa180 – 220 / 90 – 120 MPa
Poisson’s ratio νLT——0.25 – 0.33
Density / longitudinal expansion coefficient——1.8 – 1.9 g/cm³ / 8 – 10 ×10⁻⁶ /°C

The EL/GLT ratio of composite angle is about 7 to 8 (steel ≈ 2.6); this low shear modulus is the main reason FRP angle is sensitive to torsional buckling in compression (Formula 8). Values are typical ranges of the FRP and GFRP composites industry and are not NABAK COMPOSITE’s own laboratory results.

Composite angle compared with steel and aluminium angle

Table 5 — FRP angle vs S235 steel angle and 6063-T6 aluminium angle
FeatureGFRP angleSteel angleAluminium angle
Weight 50×50×5 (kg/m)0.883.771.28
Modulus E / shear modulus G (GPa)23 / 3210 / 8170 / 26
Behaviour up to failureLinear elastic, brittleDuctileDuctile
Corrosion in chemical and marine environmentsNoneSevereModerate
Electrical conductivityInsulatingConductiveConductive
Suitability for tension members and connectionsVery suitableVery suitableVery suitable
Suitability for long compression membersLimited (buckling)GoodModerate

Resin, colour and length of FRP angle

Table 6 — Ordering options for composite angle
OptionChoicesRemarks
ResinIsophthalic / vinyl ester / fire-retardantVinyl ester for severe chemical environments; fire-retardant to ASTM E84 ≤ 25
ColourYellow, grey, green, cream, black, custom RALPigment through the thickness of GFRP angle
Length6 m standard; up to 12 m and cut to sizeFactory cutting and drilling to drawing

Back-to-back double angle: two composite angles stitched together with spacers and bolts form a symmetric section that removes the weak v-axis and the torsional buckling of a single angle. For truss members and long compression braces, use FRP double angles or composite tube instead of a single angle.

FRP / GFRP Angle Profile — Technical Data SheetSection property formulas for angles | Page 4 of 5

Section formulas for composite angle

1. Cross-section area and weight
A = t ( B + b − t ) ,   w = ρ · A

50×50×5: A = 5 × 95 = 475 mm²; w = 1.85 × 475 × 10⁻³ ≈ 0.88 kg/m

2. Centroid of an equal-leg angle
e = b² + b t − t²2 (2b − t)

50×50×5: e = (2500 + 250 − 25) / 190 ≈ 14.3 mm from the back of each leg

3. Moment of inertia about the geometric axis (rectangular parts)
Ix = Σ ( bi hi³12 + Ai (yi − e)² )

The angle is divided into two rectangles b×t and t×(b − t). 50×50×5: Ix ≈ 1.13×10⁵ mm⁴

4. Product of inertia
Ixy = Σ Ai (xi − ex)(yi − ey)

For an angle Ixy is not zero, i.e. the x and y axes are not principal axes. 50×50×5: |Ixy| ≈ 6.6×10⁴ mm⁴

5. Principal moments of inertia (Mohr’s circle)
Iu,v = Ix + Iy2 ± √( ( Ix − Iy2 )² + Ixy² ) ,   tan 2θ = −2 IxyIx − Iy

For an equal-leg angle θ = 45° and Iu,v = Ix ± |Ixy|. 50×50×5: Iu ≈ 1.79×10⁵ and Iv ≈ 4.59×10⁴ mm⁴. The v-axis (corner diagonal) is the weakest axis of composite angle.

6. Minimum radius of gyration
iv = √( IvA )

50×50×5: iv = √(45 900 / 475) ≈ 9.8 mm; basis of the slenderness of compression members

7. Torsion constant of an open section
J ≈ (B + b − t) · t³3

50×50×5: J = 95 × 125 / 3 ≈ 3.96×10³ mm⁴; about one hundredth of a 50×50×4 tube of similar weight (3.89×10⁵)

Angle or tube? The torsion constant of an open composite angle grows with the cube of thickness and is hundreds of times smaller than that of a closed FRP tube of the same weight. Where torsion, buckling or long compression members occur, choose composite tube; for connections, tension bracing and supports, composite angle is the right choice.

Step-by-step example — composite angle 50×50×5: Rect 1 (50×5): A₁ = 250, y₁ = 2.5 ; Rect 2 (5×45): A₂ = 225, y₂ = 27.5 → e = (625 + 6187.5)/475 ≈ 14.3 mm Ix = 50×5³/12 + 250×11.8² + 5×45³/12 + 225×13.2² ≈ 1.13×10⁵ mm⁴ Iu = 1.13×10⁵ + 6.6×10⁴ ≈ 1.79×10⁵ ; Iv = 1.13×10⁵ − 6.6×10⁴ ≈ 4.6×10⁴ mm⁴ These values appear in Table 1 and are the basis of the design formulas on page 5.
FRP / GFRP Angle Profile — Technical Data SheetCompression, tension, connection design and fabrication | Page 5 of 5

Design formulas for composite angle

8. Torsional buckling and flexural buckling about the v-axis (compression member)
σT ≈ GLT · ( tb )² ,   Pv = π² EL Iv(K L)² ,   Pa = min(σT A, Pv, σc A)FS
Example — compression brace FRP angle 50×50×5, G = 3 GPa, E = 23 GPa, FS = 2.5: Torsional: σT = 3000 × (5/50)² = 30 MPa → PT = 30 × 475 ≈ 14.3 kN L = 1.5 m: Pv = π² × 23 000 × 45 900 / 1500² ≈ 4.6 kN → governs → Pa ≈ 1.9 kN L = 0.6 m: Pv ≈ 28.9 kN → torsional governs → Pa ≈ 14.3 / 2.5 ≈ 5.7 kN The torsional buckling stress of composite angle (30 MPa) is only about 12% of the material’s compressive strength — the key design point for FRP angle in compression. Thicker legs (larger t/b) or back-to-back double angles reduce this limitation.
9. Tension member connected by one leg (shear lag)
Ae = U · An ,   U = 1 − x̄Lc ,   Ta = Ae · σtFS

50×50×5 with 2 M10 bolts (11 mm holes) at 50 mm: An = 420, x̄ = 14.3, U ≈ 0.71 → Ae ≈ 300 mm² → Ta ≈ 300 × 240 / 2.5 ≈ 28.8 kN

10. Bolt bearing and minimum distances
Pbr = n d t σbrFS ;   e1 ≥ 2d, e2 ≥ 1.5d, p ≥ 4d

2 M10 bolts in a 5 mm leg, σbr = 150 MPa, FS = 3 → Pbr = 5.0 kN; in composite angle the connection is usually governed by bolt bearing.

11. Local buckling of the free leg (simplified)
σcr ≈ 0.425 π² E12(1 − ν²) ( tb′ )²

b′ = b − t/2. Isotropic relation; for orthotropic FRP profiles, Formula 8 (dependent on G) is more conservative and governs.

12. Eccentric load on a clip angle
M = V · ec ,   σ = 6 Mw · t²

Clip angle 76×76×9.5, length w = 150 mm, V = 5 kN, ec = 40 mm: σ = 6 × 200 000 / (150 × 90.25) ≈ 88.6 MPa; below the 100 MPa transverse flexural strength, but FS ≈ 1.1 is low → thicker leg or longer w

Fabrication guide for composite angle

  1. Cutting: cut FRP angle with a diamond or carbide saw blade at low feed pressure so the edge does not delaminate.
  2. Drilling: use a carbide drill, hole 1 to 1.5 mm larger than the bolt, observing the distances of Formula 10.
  3. Sealing: coat cut surfaces and holes with compatible resin so fibres are not exposed to moisture.
  4. Connection: stainless or FRP bolts with wide washers; in critical joints, structural epoxy adhesive together with bolts.
  5. Load direction: apply the main load along the fibre direction; limit transverse bending of the leg and the angle corner.
  6. Safety: mask, goggles and gloves when cutting and drilling; collect fibre dust with extraction.
Request a quote for FRP angle: send leg size and thickness, length and number of bars, colour, resin type and the cutting and drilling drawing.
Nabak Saze Gostar | nabakcomposite.com | +98 21 4881 2124 | Mobile +98 912 396 3078 | Instagram @nabak.composite

Disclaimer: The information in this data sheet is based on general, typical data of the FRP and GFRP composites industry and the EN 13706 standard, and is intended as guidance only. Examples are for illustration; structural design must be carried out by a qualified engineer. NABAK COMPOSITE reserves the right to change technical specifications without notice.